Products List
OthersLocation on: HOME > Products>Others
  • Brazing rings



    If you have any question,Please call us: jim@fluorotech.com.cn





  

brazing seam and lower melting point.The heating speed should be as quick as possible while brazing.The joint is to be bright grey and will return to the original color of bronze while dipped into 10% sulphuric acid.

alloy   
Corresponding     
alloy  
Ag%
P %
Sn
%
 Cu%
Solidus
Liquidus
JAgP-2
China:BCu91PAg
Japan:TC-312
America:BCuP-6
1.8-2.2
6.8-7.5
0    
The rest
1190/643   
1455/790   
JAgP-5
China:BCu88PAg
Japan:TC-315
America:BCuP-7
4.6-5.2
6.5-7.0
0
The rest
1190/643
1445/785
JAgP-6
China:BCu87PAg
America:BCup-4
5.8-6.2
6.8-7.5
0
The rest
1190/643
1370/745
JAgP-15
China:BCu80PAg
America:BCuP-5
14.5-15.5
4.8-5.3
0
The rest
1190/643
1470/800
    Lated products :